Noanix Corporation En

TECHNICAL OVERVIEW​

FT-IR

1, 10, 20, 30 : number of friction tests

The coating durability is excellent because there is little change in the FT-IR graph during 1 to 30 times of the friction test for products coated with HA Coatings .

There is little change in FT-IR graph during 1 to 20 times of friction test for products coated with PVP coatings, so the coating durability is good.

1, 10, 20, 30 : number of friction tests